This bulk concentrate is separated into 74–78% lead and 55–58% zinc concentrates, the lead being cleaned in the fourth line of cells. To handle higher-grade feed, North decided to increase flotation retention time by replacing the existing cells with 22 larger Svedala (now Minerals) Sala RCS cells, so avoiding the need to build new space.